Ashley Polymers Ashlene® 1021 Polycarbonate
Subcategory: Polycarbonate; Thermoplastic
Key Words: PC; Ashley Polymers, Inc.
Material Notes: A general purpose injection molding grade, natural resin. Also available as: 1021R (with release), 1023 (with UV stabilizers); 1023R (with release and UV stabilizers).Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|