Ashley Polymers Ashlene® 279 PPO Alloy
Subcategory: Polyphenylene Ether/PPO; Thermoplastic
Key Words: Polyphenylene Oxide; Ashley Polymers, Inc.
Material Notes: A general purpose, paintable injection molding grade with high chemical resistance and mechanical performance. Good heat resistance with dimensional stability in dark gray or black only.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |