NCMT NanoPAC™ S216 High Performance Polypropylene Nanocomposite
  Subcategory: Polypropylene; Thermoplastic 
Key Words: S Series 
Material Notes:  Characteristics: - High stiffness 
 - Supplementary of ABS 
 - Good impact resistant 
 - Less shrinkage 
 - Good thermal conductivity 
 
 Applications:  Information provided by Nano Composite Materials Technology Limited  
  
  
    | Available Properties | 
   
    
    - Density
 
- Melt Flow
 
- Tensile Strength, Ultimate
 
- Elongation at Break
 
- Tensile Modulus
 
- Izod Impact, Notched
 
- Maximum Service Temperature, Air
 
 
   |   
   |   
 | 
   | 
  
  