ND INDUSTRIES Permanent StudGrade HD 146 Threadlocker
Subcategory: Thermoset
Close Analogs: Meets military spec MIL-S-46163 Type I Grade L
Material Notes: General Description High strength, high viscosity threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Uses Fasteners over 1" diameter with coarse threads
| Available Properties |
- Viscosity
- Impact Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Cure Time
- Color
- Gap Fill, in.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|