Noble Polymers Forte™ 4CPP093 Nanocomposite
Subcategory: Polypropylene; Thermoplastic
Material Notes: Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applications replacing talc-filled, glass-filled or virgin polypropylene.Information provided by Noble Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Tangent Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
- Middle Barrel Temperature
|
|
|
|
| Property Data |