Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D
Subcategory: Polyurethane, TS; Thermoset
Material Notes: This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contact and high elongation with high energy properties. Possible applications for this material include roller skate wheels, bumpers, abrasion resistant liners and parts, rock/sand sizing screens and other specialty applications. This is a conventional “full-prepolymer” type material cured with 1,4 BDO. Can be approved for FDA dry food contact. Information provided by Northstar Polymers.
| Available Properties |
- Viscosity
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Rebound
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Maximum Service Temperature, Air
- Processing Temperature
- Mold Temperature
- Cure Time
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|