Northstar Polymers MSB-D60A High Performance Polyurethane Cast Elastomer System
Subcategory: Polyurethane, TS; Thermoset
Material Notes: This is an Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires some lord bearing, high tensile strength, cut/tear resistance, dry-abrasion resistance, and low energy rebound/response. Ester base systems are generally less expensive than PTMEG base material. Possible applications for this material include buckets/flights for conveyers, abrasion resistance liners and parts, and other specialty parts. This is a conventional “full-prepolymer” type material cured with 1,4 BDO. Can be approved for FDA dry food contact. Information provided by Northstar Polymers.
| Available Properties |
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Rebound
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Maximum Service Temperature, Air
- Processing Temperature
- Mold Temperature
- Cure Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|