NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin
Subcategory: Polyethylene; Thermoplastic; MDPE
Material Notes:
Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals
| Available Properties |
- Density
- ESCR 100% Igepal®
- ESCR 10% Igepal®
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|