INEOS NOVA Zyntar® 7000 Flame Retardant Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: Features:General purpose workhorse resinGood flow for injection moldingUL94 V-0 @ 1.5 mm for all colors UL94 5VA rating FOAMED @ 4.6 mm, 0.87-1.07 g/cc density, natural colorCustom colors availableApplications: - Television cabinets (front bezel, TV backs)
- Consumer electronics
- Exercise equipment
- Business equipment
Information provided by Nova Chemicals.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|