INEOS NOVA 3590 General Purpose Crystal Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: This grade no longer in product line. INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Key Words: GPPS
Material Notes: Excellent blending resin, Suitable for difficult to fill and thin wall molding, Low residuals, USP Class VI Applications: Blending applications, Single service drinkware, Medical molding Exposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical properties of the material. Properties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Refractive Index
- Optical Density
- Transmission, Visible
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|