|   INEOS NOVA 4211 Medium Impact Polystyrene  Subcategory: Polystyrene; Thermoplastic Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.  Material Notes: Excellent balance of properties, USP Class VI
 Applications: Consumer electronics, Injection molding applications Properties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified. Information provided by NOVA Chemicals. 
| | 
    | Available Properties |  
    | DensityLinear Mold ShrinkageMelt FlowTensile Strength, YieldElongation at BreakModulus of ElasticityFlexural ModulusFlexural Yield StrengthIzod Impact, NotchedDielectric ConstantDielectric StrengthDeflection Temperature at 1.8 MPa (264 psi)Vicat Softening PointFlammability, UL94Melt TemperatureMold Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |