INEOS NOVA S-4600 High Impact Compact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: High impact polystyrene with excellent flow characteristics, a very high toughness and a high elongation. Main application are injection molding of technical parts and housings. For injection molding generally a lubricated type is used. All mechanical properties measured under standard conditions 50% RH and 23°C. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- CTE, linear 20°C
- Thermal Conductivity
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|