INEOS NOVA S-6600 High Impact Compact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: High impact polystyrene which is very easy processed in extension and thermoforming processes. Typical applications are packaging of food stuffs like Yogurt beakers but technical parts and extruded profiles are easily processed too. For injection molding generally a material with better flow characteristics and a lubricated type is used. All mechanical properties measured under standard conditions 50% RH and 23°C. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- CTE, linear 20°C
- Thermal Conductivity
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|