INEOS NOVA S-6600MG Compact Polystyrene Microgranulates
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: High impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm especially useful for compounding and extrusion applications. Due to the higher viscosity intensive mixing with thermoplastic elastomers is possible leading to more homogeneous end-products. IT is also very suitable for the production of extruded foils and sheets. All mechanical properties measured under standard conditions 50% RH and 23°C. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- CTE, linear 20°C
- Thermal Conductivity
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|