NOVA Chemicals Sclair® 11H1 LLDPE Film Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Low gel, Excellent heat sealability, Easy processability, High toughness and strength Applications: Heavy duty sack, High strength packaging Additives: Process stabilizer, Polymer process aid, Antiblock Canada: The Health Protection Branch has indicated no objection to the sue in Canada of this resin for a variety of food packaging applications. Information on the packaging of specific foodstuffs should obtained from NOVA Chemicals or from the Health Protection Branch, Food Packaging Materials and Incidental Additives Section, Ottawa, Canada. United States: This resin complies with the specification contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymer, para. (c) 3.2a, and ay thus be sued in the United States as an article or component of an article intended for use in contact with food. Other Countries: For regulatory compliance information for other countries, please contact your nearest NOVA Chemicals office. Film properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are dependent upon operating conditions. Information provided by NOVA Chemicals.
Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Haze
- Gloss
- Melt Temperature
- Die Opening
- Blow Up Ratio
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
|