NOVA Chemicals Sclair® 2607-UV14 HDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Excellent stiffness, Good impact resistance, Low warpage Applications: Roll-out carts Additives: Elevated levels of ultraviolet stabilizer packages, Elevated levels of antioxidants Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Vicat Softening Point
- Melt Temperature
|
|
|
|
| Property Data |