NOVA Chemicals Sclair® 56B4 HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Extra-high stress crack resistance, Good processability Applications: Very high ESCR, Ideally suited for use in most food, pharmaceutical, households and industrial chemical applications, Little/no stacking Additives: Processing A/O, Available in a UV-stabilized version, A high-antioxidant version (56B4) is available where extra stabilization is required Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Melt Temperature
|
|
|
|