NOVA Chemicals Novapol® HB-W646-A HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: High molecular weight HDPE, Excellent ESCR, Impact strength, Good processability Applications: Drums, Jerry cans, IBCs, Marine fuel tanks Additives: Process stabilizer Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Brittleness Temperature
- Melt Temperature
|
|
|
|
| Property Data |