NOVA Chemicals Novapol® HD-2079-BK HDPE Pipe Coating Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Medium molecular weight HDPE, High ESCR, Good toughness, Good chemical resistance, Good processability, Excellent UV stability Applications: Extrusion onto metal pipe to produce a corrosion-resistant coating for buried pipe systems, Wide range of profile extrusions, Sheet extrusion for thermoforming, Corrugated tubing, Conduit Additives: Antioxidants, Carbon black Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Water Absorption
- Environmental Stress Crack Resistance
- Oxidative Induction Time (OIT)
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
- Filler %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|