NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffness Applications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert and conduit application Additives: Antioxidants and processing stabilizers Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Vicat Softening Point
- Brittleness Temperature
- Melt Temperature
|
|
|
|