NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Film
Material Notes: Excellent stiffness, Moderate toughness, Easy processability Applications: Industrial packaging, Liners, Blends with LLDPE, Foam articles Additives: Base resin Film properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are dependent upon operating conditions. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Haze
- Gloss
- Melt Temperature
- Blow Up Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|