NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: Excellent ESCR, Excellent toughness, High strength, High flexibility Applications: Pipes for pressure and non-pressure service from 12 mm to 100 mm, Potable water pipe and tubing, Underground sprinkler systems, Irrigation pipe Additives: Antioxidants and processing stabilizers Pipe properties: 1 in nominal diameter laboratory pipe SDR 13.5. Long-Term Hydrostatic Strength, Nominal: 5.5 MPa, as per ASTM D746. Compressed Ring ESCR, F50: 2500 hours minimum as per ASTM D1248. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|