NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin
Subcategory: Polyethylene; Thermoplastic; MDPE
Material Notes: Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61 Applications: Toys, General purpose custom molding, Carts, Playground equipment Additives: Process stabilizer, UV stabilizer Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
|
|
|
|