NOVA Chemicals Sclair® SD-7250-0B HDPE Extrusion Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Good adhesion, Excellent barrier properties, Good heat resistance Applications: Silicon-coated release papers, Composite can liners, Base coat for photographic papers, Snack food packaging Additives: Antioxidant Heat Seal Temperature: 135°C , minimum value, 1-mil coating on kraft paper Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Melt Flow
- Neck In
- Drawdown
- Coating Weight
- Coefficient of Friction
- Melting Point
- Vicat Softening Point
|
|
|
|