NOVA Chemicals Sclair® 8107 UV8D Butene LLDPE Rotational Molding Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listed Applications: Food and laundry materials handling, IBCs, Chemical containers, Parts requiring flat surfaces or low shrinkage characteristics, Intricate custom parts Additives: Processing antioxidants, UV stabilizers Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Ultimate
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|