NOVA Chemicals Novapol® TR-0338-UI Hexene MDPE Rotational Molding Resin
Subcategory: Polyethylene; Thermoplastic; MDPE
Material Notes: Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing window Applications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, Agricultural storage tanks Additives: Processing antioxidants, UV stabilizers Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Ultimate
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |