INEOS NOVA 782 High Performance Styrenic Enhanced Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: This grade no longer in product line. INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: High flow, Custom colors Applications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripherals Performance grades of polystyrene are engineered to have specific properties. These products can be custom colored. NOVA Chemicals can accurately match your color needs with its leading edge color technology. Injection Speed: Fast Colored material may differ in some properties. All molded samples were an 1/8 inch thick unless noted. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|