NOVA Chemicals Styrocell® B733A Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: Expanded Polystyrene, EPS
Material Notes: This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the production of cellular bricks. Applications: This grade is used to produce cellular bricks from a mixture of pre-expanded beads with clay, which are subsequently fired in a kiln at ca. 1000°C. This grade should not be used for food contact applications. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Bulk Density
- Bead Size
- Styrene Content
- Blowing Agent Content
|
|
|
|