NOVA Chemicals D175B Fast Cycle Shape Grade Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: December 2003: This datasheet is obsolete.
Key Words: Expanded Polystyrene, EPS
Material Notes:
Applications: General shape market Expansion: Minimum Density Potential: 1.20 pcf (continuous); 1.05 pcf (batch) Characteristics: Typically Lump Free Prepuff Flow: Dry, Free-Flowing Expected Federates: Average Bead Size: Intermediate "B" grade; 96% through 16 on 30 U.S. Standard sieve Molding Range: Wide Cycle Speed: Fast Part Appearance: Good Age Time Before Molding: 16 to 24 hours Comments: Easy molding material Information provided by NOVA Chemicals.
|
|
|