NOVA Chemicals D185B Regular Expandable Polystyrene
  Subcategory: Polystyrene; Thermoplastic 
Close Analogs: December 2003:  This datasheet is obsolete. 
Key Words: Expanded Polystyrene, EPS 
Material Notes: 
  Applications: Custom molding - Fast cycle packaging Expansion: Minimum Density Potential: 1.10 pcf (continuous); 1.30 pcf (batch) Characteristics: No Lumping Prepuff Flow: Average Expected Federates:  Average Comments: Expands well Bead Size: "B" 96% through 16 on 30 U.S. Standard Sieve Molding Range: Variable Cycle Speed: Very Fast Part Appearance: Acceptable for packaging, not for cooler applications Age Time Before Molding: 2 to 36 hours Comments: Consistently fast cycling; Excellent for vacuum equipment Information provided by NOVA Chemicals. 
| 
  
 | 
   | 
  
  
    | Property Data | 
   
    