NOVA Chemicals D185B Regular Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: December 2003: This datasheet is obsolete.
Key Words: Expanded Polystyrene, EPS
Material Notes:
Applications: Custom molding - Fast cycle packaging Expansion: Minimum Density Potential: 1.10 pcf (continuous); 1.30 pcf (batch) Characteristics: No Lumping Prepuff Flow: Average Expected Federates: Average Comments: Expands well Bead Size: "B" 96% through 16 on 30 U.S. Standard Sieve Molding Range: Variable Cycle Speed: Very Fast Part Appearance: Acceptable for packaging, not for cooler applications Age Time Before Molding: 2 to 36 hours Comments: Consistently fast cycling; Excellent for vacuum equipment Information provided by NOVA Chemicals.
|
|
|