NOVA Chemicals D240B Regular Low Pentane Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: December 2003: This datasheet is obsolete.
Key Words: Expanded Polystyrene, EPS
Material Notes:
Applications: Low pentane, high strength shape molding Expansion: Minimum Density Potential: 1.80 pcf (continuous); 1.10 pcf (batch) Characteristics: No lumping Prepuff Flow: Dry, Free-Flowing Expected Federates: Note Densities Bead Size: Intermediate "B" size Molding Range: Wide Cycle Speed: Moderately Fast Part Appearance: Excellent Age Time Before Molding: 4 to 36 hours Comments: An easy material to mold; Excellent fusion and molded part strength Information provided by NOVA Chemicals.
|
|