NOVA Chemicals D244B Low Pentane Regular Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: Expanded Polystyrene, EPS
Material Notes:
Applications: Low pentane, fast cycle shape molding Expansion: Minimum Density Potential: 1.30 pcf (continuous); 1.90 pcf (batch) Characteristics: No lumping, No static Prepuff Flow: Dry, Free-Flowing Expected Federates: Note Densities Bead Size: Intermediate "B" size Molding Range: Medium Cycle Speed: Very Fast Part Appearance: Good Age Time Before Molding: 4 to 24 hours Comments: A very fast cycling material with good fusion and molded part appearance Information provided by NOVA Chemicals.
|
|
|