NOVA Chemicals D64B Regular Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: December 2003: This datasheet is obsolete.
Key Words: Expanded Polystyrene, EPS
Material Notes:
Applications: Shape, Custom, Packaging, Block, Floatation Expansion: Minimum Density Potential: 1.30 pcf (continuous); 1.10 pcf (batch) Characteristics: No lumping Prepuff Flow: Average Expected Federates: 600-800 pph in 250 gal. expander Bead Size: "B" - 96% through 16 on 30 U.S. standard mesh Molding Range: Variable, easy to mold Cycle Speed: Fast at lower densities; Long at 1.50 pcf and above Part Appearance: Excellent Age Time Before Molding: 4 to 24 hours Comments: Very versatile material for custom and block Information provided by NOVA Chemicals.
|
|
|