INEOS NOVA Dylark® 378P20 High Performance Glass Filled Styrenic
Subcategory: Polystyrene; Thermoplastic; Polymer
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethane Applications: Instrument panel substrates, consoles, Cluster housing, interior trim Injection Speed: Medium-Fast Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Poissons Ratio
- Izod Impact, Notched
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Processing Temperature
- Melt Temperature
- Mold Temperature
- Back Pressure
- Screw Speed
- Filler %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|