NOVA Chemicals Dytherm® 140R Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: Expanded Polystyrene, EPS
Material Notes: This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved thermal resistance. Applications: This grade is used for medium density foam with improved thermal resistance. Typical applications include hot water insulation and automotive parts (interior and exterior). Processing of DYTHERM beads on pressurized batch pre-expanders is recommended. DYTHERM 140R can be processed on a continuous pre-expander when high densities are acceptable. Detailed processing advice is given in the DYTHERM bulletins, available from your local NOVA Chemicals company. This grade should not be used for food contact applications. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Bulk Density
- Bead Size
- Styrene Content
- Blowing Agent Content
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|