NOVA Chemicals Styrocell® EF443C Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: Expanded Polystyrene, EPS
Material Notes: This is a fire retardant molding grade typically used for medium-density foam applications. It consists of spherical polystyrene particles (beads) containing an expanding agent, pentane and an internal flame retardant additive. Applications: This is a fire retardant molding grade. It is used for the producing block at medium densities, which are subsequently cut into board. Compared with standard Styrocell grades, EF443C offers more controllable pre-expansion, short maturing times and fast cycle time during molding. This grade should not be used for food contact applications. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Bulk Density
- Bead Size
- Styrene Content
- Blowing Agent Content
- Reaction to Fire
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|