NOVA Chemicals Styrocell® F443C Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: Expanded Polystyrene, EPS
Material Notes: A fast cycling fire retardant molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, and an internal flame retardant additive. It is typically for molding medium/medium density foam. Applications: This is used mainly for producing low/medium density block which is cut to make insulation board. This grade should not be used for food contact applications. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Bulk Density
- Bead Size
- Styrene Content
- Blowing Agent Content
- Reaction to Fire
|
|
|
|