NOVA Chemicals Gedexcel® 44B Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: Expanded Polystyrene, EPS
Material Notes: Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, and from 23* kg/m³ with the use of under pressure discontinuous expanders. Information provided by NOVA Chemicals.
|
|
|
| Property Data |