NOVA Chemicals M77A Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: December 2003: This datasheet is obsolete.
Key Words: Expanded Polystyrene, EPS
Material Notes:
Applications: Block, Insulation, Roofing Expansion: Minimum Density Potential (pcf): 1.05 pcf (Continuous) Characteristic of no lumping. Prepuff Flow is dry, and free-flowing. Expected Federates (pph): Excellent Typically good feedrates and consistent density control Bead Size: "A"-96% through 10 on 25 U.S. Standard Sieve Molding Range: Wide Cycle Speed: Fast Part Appearance: Very Good Age Time Before Molding: 24 to 48 hours
Information provided by NOVA Chemicals.
|
|
|