INEOS NOVA M97B Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: December 2003: This datasheet is obsolete.
Key Words: Expanded Polystyrene, EPS
Material Notes:
Applications: Roofing, Fabricating, Custom Molding Expansion: Minimum Density Potential (pcf): Batch1.05 pcf; Continuous 1.2 pcf Characteristic of typically lump free and no static Prepuff Flow is dry, and free-flowing. Expected Federates (pph): Average Expansion is typically problem free with consistent density Bead Size: "B"-96% through 16 on 30 U.S. Standard Sieve Molding Range: Wide Cycle Speed: Fast Part Appearance: Good-Excellent Age Time Before Molding: 4 to 24 hours
Information provided by NOVA Chemicals.
|
|
|