INEOS NOVA N2000MG Compact PS
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: Very easy flowing general purpose polystyrene Microgranulates, having a diameter of 0.5-0.7 mm. As the specific surface area is very large, Microgranulates are well suited for compounding purposes. Due to high flow the filler load may be very high while the processing requires only a minimum of energy. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- CTE, linear 20°C
- Thermal Conductivity
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|