INEOS NOVA N3301M Compact PS
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: Very easy flowing general purpose polystyrene , designed for standard injection molding applications of thin walled articles where an optimal combination of dimensional stability, flow characteristics and mechanical properties are required. Most applications are in the production of crystal clear disposables, household goods, cups, toys, etc. and as a gloss-layer-layer on extrudes sheet. For injection molding generally a lubricated grade is used. Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- CTE, linear 20°C
- Thermal Conductivity
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|