INEOS NOVA N9400M Compact PS
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: N9400M is transition material from the mass units, produced during change over from one grade to another. N9400M is plasticizer containing transition material. As a consequence the Vicat temperature is below 98°C. The data-ranges which are given can just be used as an indication. In practice the range will be much smaller Information provided by NOVA Chemicals.
| Available Properties |
- Melt Flow
- CTE, linear 20°C
- Vicat Softening Point
|
|
|
|
| Property Data |