INEOS NOVA N9900M Compact PS
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: N9900M is an "undefined" PS start-up material from starting up the extruder. As a consequence burned material and high styrene monomer content is part of the composition of the material. Since is can be start-up material from any GPPS grade, properties like melt index, Vicat, etc., can vary. Information provided by NOVA Chemicals.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|