INEOS NOVA NAS® 90 High Performance Styrenic
Subcategory: Polystyrene; Thermoplastic
Close Analogs: INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets.
Material Notes: NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Plastics. It also has good gamma radiation resistance and has a UL94 HB rating at 1.5 mm for uncolored materials. Applications: Appliances, point-of-purchase displays, housewares, bathroom accessories, medical devices, and toys Information provided by NOVA Chemicals.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Unnotched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Refractive Index
- Haze
- Transmission, Visible
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|