NOVA Chemicals P743C Expandable Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam. Applications: Styrocell P743C is used mainly for producing contour moldings with wall thickness less than 10 mm. This grade complies with major European and US food contact regulatory regimes, including: European Community Directive 90/128/ECC, including 92/39EEC and 95/EC, relating to plastics materials and articles, intended to come into contact with foodstuffs. Information provided by NOVA Chemicals.