Noveon ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic
Subcategory: Elastomer, TPE; Thermoplastic; Polymer
Material Notes: Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extension to the Noveon Estane® TPU technology, Estaloc® RETP products complement Estane's durability and aesthetics with increased stiffness capability and dimensional stability over a broad temperature performance range not available from other engineering thermoplastics.Major Benefits of Estaloc® RETPs: - Superior Dimensional Stability approaching that of metals
- Class A surface aesthetics
- Paintability with no primer nor adhesion promoter
- Excellent abrasion and scuff/mar resistance
- Extraordinary toughness over a broad temperature range
- Excellent adhesion to a variety of overmolding chemistries
Specific Notes for this Material: Fiberglass reinforced TPU - industry standard for recreational wheel hubs Information provided by Noveon, Inc.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched @ -40°C
- CTE, linear 68°F
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|