Noveon Hipscon™ M-520 Static Control High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: Hipscon™ M-520 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are easily formed into deep pockets that maintain uniform static protection and show excellent "crush strength." Hipscon maintains extremely low gloss surfaces after forming, allowing for easy reading of package contents via automated sensors. Hipscon™ M-520 sheet is available in custom extruded gauges from 0.012 to 0.080 inch and widths of 10 to 48 inches. Product is typically provided as rollstock with a smooth surface finish. Features: - Superior crush strength
- High degree of stiffness
- Uniform pocket formation
- Consistent, permanent ESD protection
Applications: - Electronic component packaging and handling trays
- Tape & reel
- Material handling boxes and bins
Data provided by Noveon, Inc.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Volume Resistivity
- Surface Resistance
- Static Decay
- Deflection Temperature at 1.8 MPa (264 psi)
- Gloss
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|