Noveon STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Material Notes: Description: Inherently dissipative, this patented technology delivers surface resistivity in the range of 10E8 to 10E10 O/square. Stat-Rite® IDP Polymers forms a molecular-scale, interpenetrating polymer network which carries charge. The polymeric charge carriers are permanent over time even through customer processing in injection molding or extrusion. The fundamental Estane® TPU backbone dominates in property performance. Stat-Rite® IDP (Inherently Dissipative Polymer) is a homogeneous polymer which lends itself to consistent voltage decay throughout the matrix of a finished product. Conversely alternative technologies including the use of fillers or additives can off-gas, migrate, or slough-off causing contamination at a minimum and slow or inconsistent ESD protection. Stat-Rite® IDP Elastomer Alloys are based upon TPU providing the ultimate mechanical durability, low temperature flexibility and permanent ESD protection.Major Benefits of Stat-Rite® IDP Elastomer Alloys: - Permanent static dissipation
- Ultra-clean
- Low off-gassing; low ionics
- Clarity
- No particulates
- TPU performance
Applications: - Clean room soft walls, windows, and doors
- Materials handling hose and tubing
- Vacuum hose and tubing
- Work surface mats
Specific Notes for this Material: Permanent Electrostatic Dissipation (ESD) without carbon or anti-stats Information provided by Noveon, Inc.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Volume Resistivity
- Surface Resistivity per Square
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|